The pore size of 4A molecular sieve is 4A. It is mainly used to adsorb water, methanol, carbon dioxide, ethylene, propylene, does not adsorb any larger molecular than 4A and often used as desiccant in industrials.
Item |
Unit | Type | |||
Shape | Pellet | Sphere | |||
Diameter | mm | 1.5 - 1.7 | 3.0-3.3 | 1.7-2.5 | 3.0-5.0 |
Size ratio up to grade | % |
≥98 |
≥98 | ≥96 | ≥96 |
Bulk Density | g/ml | ≥0.60 | ≥0.60 | ≥0.64 | ≥0.64 |
Wear Ratio | % | ≤0.20 | ≤0.25 | ≤0.20 | ≤0.20 |
Crushing Strength | N | ≥30/cm | ≥45/cm | ≥60/p | ≥70/p |
Static Adsorption | % | ≤16 | ≥16 | ≤16 | ≤16 |
Packing Water | % | ≤1.5 | ≤1.5 | ≤1.5 | ≤1.5 |